Polymer Property : Peel Strength = 5.30 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 5.30 kN/m
30.2 pli
ASTM D-1876-72
Lubrizol ESTANE® 5713 Ester Based Thermoplastic Polyurethane
Features: It has the highest heat resistance of any Estane TPU resin used in adhesives. Supplied as pale amber granules, it is soluble in THF or THF/MEK blends. Higher heat resistance, tensile and b..