Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.900 kN/m | 5.14 pli | Aluminum Foil; ASTM D1867-72 |
Lubrizol ESTANE® 5701 Ester Based Thermoplastic Polyurethane Features: Displays Low Temperature Flexibility and Abrasion Resistance.Uses: Audio Tape Binder and Screen Printing Inks, Inks and Lacquers, Cast Film for LaminationAvailable in Americas and AsiaInfo.. |