Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.06 - 5.10 kN/m | 17.5 - 29.1 pli | Initial (5 min.) PVC vs. PVC |
Taiwan Sheen Soon Sheenthane® AS-420 TPU for PU Adhesive Thermoplastic polyurethane elastomer for solvent-based polyurethane adhesive.Hydrolysis resistance gradeExcellent bonding strength for polyester, TPU, nylon, PVC, leather, fabrics, etc. Used for fo.. |