Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 80.0 kN/m | >= 456 pli | 80+5°C; ISO 21809-1 |
Lushan L-5R (HC) Polyethylene Copolymer Adhesive for Steel Pipe Coating Copolymer adhesive resin Lushan L-5R series is maleic anhydride grafted polyethylene which could be in granule or powder form. It was developed by Lushan with independent patent technologies and pro.. |