Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 4.19 kN/m | 23.9 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 55580R028 0.028" (0.711 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum on fiberglass clothThis data represents typical values for th.. |