Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 4.15 kN/m | 23.7 pli | |
Valley Adhesives EM-422 High Temperature Application Glue Stick Valley Adhesives EM-422 High Temperature Application Glue StickRapid strength build up; Excellent hot tacking and wetting; Bonds corrugated boxes and paper in packaging operations and repackaging ar.. |