Mechanical Properties Metric English Comments
Peel Strength 0.7175 kN/m

@Treatment Temp. 74.0 °C,
Time 173000 sec
4.094 pli

@Treatment Temp. 165 °F,
Time 48.0 hour
95% RH, To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4000 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Peel Strength 0.7175 kN/m

@Treatment Temp. 74.0 °C,
Time 173000 sec
4.094 pli

@Treatment Temp. 165 °F,
Time 48.0 hour
95% RH, To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4002 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Peel Strength 0.7175 kN/m

@Treatment Temp. 74.0 °C,
Time 173000 sec
4.094 pli

@Treatment Temp. 165 °F,
Time 48.0 hour
95% RH, To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4004 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Peel Strength 0.7175 kN/m

@Treatment Temp. 74.0 °C,
Time 173000 sec
4.094 pli

@Treatment Temp. 165 °F,
Time 48.0 hour
95% RH, To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4006 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..
Peel Strength 0.7175 kN/m

@Treatment Temp. 74.0 °C,
Time 173000 sec
4.094 pli

@Treatment Temp. 165 °F,
Time 48.0 hour
95% RH, To Aluminum; ASTM D1000
Parker Chomerics SOFT-SHIELD® 4008 Low Closure Force, Foam Core EMI Gasket
Description: Chomerics’ SOFT-SHIELD 4000 Series materials are low-cost, low closure force EMI gaskets that provide effective shielding and grounding of commercial electronic devices, indoor enclosu..