Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.500 - 35.0 kN/m | 2.85 - 200 pli | Average value: 7.89 kN/m Grade Count:96 |
Overview of materials for Styrenic Elastomer (TES) This property data is a summary of similar materials in the MatWeb database for the category "Styrenic Elastomer (TES)". Each property range of values reported is minimum and maximum values of appro.. |