Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.58 kN/m | 20.4 pli | Steel coupon, 180° |
3M Scotch-Weld™ 6116 Bulk only Adhesive Same as 6111 but Lower than normal viscosity and mainly used on fabrics.Information provided by 3M |
|||
Peel Strength | 3.58 kN/m | 20.4 pli | Open weave polyester fabric, 180° |
3M Scotch-Weld™ 6116 Bulk only Adhesive Same as 6111 but Lower than normal viscosity and mainly used on fabrics.Information provided by 3M |