Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.56 kN/m | 20.3 pli | After 2 week exposure to 71°C, Vinyl-Gerfor MK foamed backed to Composite, 2 surface Bond |
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.Infor.. |
|||
Peel Strength | 3.56 kN/m | 20.3 pli | ABS Plastic, 180° |
3M Scotch-Weld™ 6116 Bulk only Adhesive Same as 6111 but Lower than normal viscosity and mainly used on fabrics.Information provided by 3M |