Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 3.14 kN/m | 17.9 pli | Bond Strength; Arlon SQA-TMS-011 |
Arlon 44580R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 1165 Fiberglass (Flexible Heater Substrate)This data represents typical values for the producti.. |