Mechanical Properties Metric English Comments
Peel Strength 4.77 kN/m
27.2 pli
1 oz EDC foil; after solder float; IPC-TM-650 2.4.8
Rogers Corporation RT/duroid® 5870 Glass Microfiber Reinforced PTFE High Frequency Laminate
RT/duroid® 5870 and 5880 glass microfiber reinforced PTFE composites are designed for exacting stripline and microstrip circuit applications. Glass reinforcing microfibers are randomly oriented to..