Polymer Property : Peel Strength = 24.2 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 4.24 kN/m
24.2 pli
Dow BETAMATE™ 73345G Epoxy
BETAMATE™ 73345G is a one-part, high performance, heat curing, epoxy adhesive. It is capable of bonding oily galvanized and cold rolled steel without a primer and has corrosion resistance. BETAMA..