Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.89 kN/m @Temperature 24.0 °C, Time 86400 sec |
16.5 pli @Temperature 75.2 °F, Time 24.0 hour |
180°, Canvas/Steel |
3M Scotch-Weld™ 4491 Vinyl Bonding Cylinder Spray Adhesive Industrial grade, high performance, plasticizer resistant bulk spray adhesive formulated for bonding vinyl. The adhesive is available in a convenient, portable, no maintenance aerosol cylinder.Infor.. |
|||
Peel Strength | 2.89 kN/m | 16.5 pli | Cold Rolled Steel, 180° |
3M Scotch-Weld™ 6111 Green Bulk only Adhesive Same as 6111 tan but green in colorInformation provided by 3M |
|||
Peel Strength | 2.89 kN/m | 16.5 pli | ABS, 180° |
3M Scotch-Weld™ 6111HT Blue Bulk only Adhesive Same as 6111 but has higher heat resistance and blue in colorInformation provided by 3M |
|||
Peel Strength | 2.89 kN/m | 16.5 pli | ABS, 180° |
3M Scotch-Weld™ 6111HT Tan Bulk only Adhesive Same as 6111 but has higher heat resistanceInformation provided by 3M |
|||
Peel Strength | 2.89 kN/m | 16.5 pli | Cold Rolled Steel, 180° |
3M Scotch-Weld™ 6111 Tan Bulk only Adhesive Sprayable 100% solventless adhesive for most foams, fabrics, plastics, particle board and thin metalInformation provided by 3M |