Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.77 kN/m | 15.8 pli | Bond Strength; ASTM D624 |
Arlon 18609R023 0.023" (0.584 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneLayer 1: Cured Silicone RubberLayer 2: Uncured Silicone RubberSubstrate: 11523 Style FiberglassThis data represents typical values for the production mate.. |
|||
Peel Strength | 2.77 kN/m | 15.8 pli | Bond Strength; ASTM D624 |
Arlon 56609R028 0.029" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production materi.. |