Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Peel Strength = 2.68 pli Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.470 kN/m
2.68 pli
to polyethylene, 180° peel test, rate of peel = 300mm/min at 25°C
Kuraray SEPTON® A3 Hot Melt Adhesive
Description: SEPTON® is a series of high performance thermoplastic rubbers developed by Kuraray Co. Ltd. Using its isoprene technology. SEPTON® resins are a series of hydrogenated styrenic blo..
Peel Strength 0.470 - 1.35 kN/m
2.68 - 7.72 pli
Average value: 0.886 kN/m Grade Count:4
Overview of materials for Thermoplastic Elastomer, Melt-Processible Rubber
This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Elastomer, Melt-Processible Rubber". Each property range of values reported is minimum and..