Peel Strength 2.44 kN/m
13.9 pli
Bond Strength; Arlon SQA-TMS-011
Arlon 51044R020 0.020" Semi-Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Semi-cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production material and should no..