Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.26 kN/m | 12.9 pli | |
Valley Adhesives EM-222 Low Temperature Application Glue Stick Valley Adhesives EM-222 Low Temperature Application Glue StickRapid strength build up; Excellent hot tacking and wetting; Safe on styrofoam and heat sensitive materials; Bonds corrugated boxes and p.. |