Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.816 kN/m | 16.06 pli | 90° Peel, PET/PET, 72 hrs at 70°C; ASTM D3330 |
3M 7997MP Hi-Performance Acrylic 200MP This adhesive meets the requirements of most long-term applications. It offers temperature resistance to 400°F (204°C). Peel adhesion values are excellent on most membrane switch substrate materia.. |