Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 2.79 kN/m @Temperature 82.0 °C, Time 14400 sec |
15.9 pli @Temperature 180 °F, Time 4.00 hour |
Aluminum, etched, Bell Peel, Adhesive Failure; ASTM D3167 |
3M Scotch-Weld™ LSB60 Toughened Epoxy Adhesives 3M™ Scotch-Weld™ Toughened Epoxy Adhesive LBS60 is a high performance, two-part, toughened epoxy adhesives offering outstanding shear adhesion and very high levels of durability with a choice of f.. |