Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | >= 15.0 kN/m | >= 85.6 pli | 3-layer; DIN 30670/NFA 49-710 |
Borealis Borcoatâ„¢ ME0433 Polyethylene Adhesive In Powder form for Steel Pipe Coating Borcoat ME0433 is a maleic-anhydride grafted polyethylene polymer with excellent adhesion to fusion bonded epoxy and the top-coat HDPE.Borcoat HE0433 is primarily designed to be used as the tie laye.. |