Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.79 kN/m | 10.2 pli | Copper; 1 oz. EDC After Solder Float; IPC-TM-650 2.4.8 |
Rogers Corporation RO3203 Woven-Glass Reinforced PTFE Laminate Features and Benefits:Woven glass reinforcement - Improves rigidity for easier handlingUniform electrical and mechanical performance - ideal for complex multi-layer high frequency structuresLow diel.. |
|||
Peel Strength | 1.79 kN/m @Temperature 288 °C, Time 10.0 sec |
10.2 pli @Temperature 550 °F, Time 0.00278 hour |
Copper, After Solder Float; IPC-TM-650 2.4.8 |
Rogers Corporation RO3035 Ceramic-Filled PTFE Composite, High Frequency Circuit Material Features and Benefits:Low dielectric lossExcellent mechanical properties versus temperature - reliable stripline and multi-layer board constructions.Uniform mechanical properties- ideal for multi-la.. |