Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.33 kN/m | 7.60 pli | 180°, Oak, 50% RH |
3M PN8017 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Peel Strength | 1.33 kN/m | 7.60 pli | 180°, Oak, 50% RH |
3M PN8019 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Peel Strength | 1.33 kN/m | 7.60 pli | 180°, Oak, 50% RH |
3M PN8027 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |
|||
Peel Strength | 1.33 kN/m | 7.60 pli | 180°, Oak, 50% RH |
3M PN8029 Marine Grade Silicone Sealant A mildew resistant, non-sagging, moisture curing silicone rubber sealant for above the waterline applications which remains flexible with excellent resistance to the marine environment. Adheres to b.. |