Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.26 kN/m
7.20 pli
To Copper (1 oz./35 micron); After Thermal Stress; IPC TM-650 2.4.8
Arlon 33N Polyimide Laminate and Prepreg
High reliability and high temperature material33N is a flame retardant polyimide laminate and prepreg system where the excellent high performance properties of polyimide need to be combined with fla..
Peel Strength 1.26 kN/m
7.20 pli
To Copper (1 oz./35 micron); At Elevated Temperatures; IPC TM-650 2.4.8.2
Arlon 33N Polyimide Laminate and Prepreg
High reliability and high temperature material33N is a flame retardant polyimide laminate and prepreg system where the excellent high performance properties of polyimide need to be combined with fla..
Peel Strength 1.26 kN/m
7.20 pli
Bond Strength; ASTM D624
Arlon R36461R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Liner: Polyethylene Side 1: Uncured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Liner: Polyethylene This data represents typical values for..