Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.175 - 0.1972 kN/m | 1.00 - 1.125 pli | Adhesion |
Dielectric Polymers NT-500 Protective Film
(discontinued **) Crosslinked silicone adhesive with electrical grade polyester film backing.Features: Clean tape removalNo film shrinkage after exposure to elevated temperaturesApplications: Used as a fume mask duri.. |