Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 1.08 kN/m | 6.16 pli | 90° Peel (Width=10) after 200°C for 7 days; IPC-FC-241B |
UBE UPISEL-N BE1210 Copper Clad Laminate Description: UPISEL-N BE1210 is non-adhesive type flexible Copper Clad Laminate (Polyimide = 25µm, Cu = 18µm) based on "UPILEX-VT." UPISEL-N has excellent dimensional stability and heat resistance.. |
|||
Peel Strength | 1.08 kN/m | 6.16 pli | 90° Peel (Width=3.2), 100% Retained with 2N-HCl or 2N-NaOH; IPC-FC-241B |
UBE UPISEL-N BE1210 Copper Clad Laminate Description: UPISEL-N BE1210 is non-adhesive type flexible Copper Clad Laminate (Polyimide = 25µm, Cu = 18µm) based on "UPILEX-VT." UPISEL-N has excellent dimensional stability and heat resistance.. |