Polymer Property : Peel Strength = 1.02 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 1.02 kN/m
5.80 pli
after solder float; IPC-TM-650.2.4.8
Park Electrochemical Nelco® N7000-2 V0 Toughened Polyimide Laminate and Prepreg
The Nelco N7000-2 V0 series is a next-generation high-Tg polyimide using a toughened resin chemistry to achieve a UL 94-V0 designation. This advanced material is designed for use in a wide variety o..
Peel Strength 1.02 kN/m
5.80 pli
Bond Strength (S1 to S1); Arlon SQA-TMS-011
Arlon 48146X008 0.0080" Cured/Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the producti..
Peel Strength 1.02 kN/m
5.80 pli
Bond Strength; ASTM D624
Arlon R34381R014 0.014" (0.356 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave 1: Polyethylene Side 1: Uncured Silicone Rubber Substrate: 7628 Style FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typical..