Polymer Property : Peel Strength = 0.298 kN/m Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Peel Strength 0.298 kN/m
1.70 pli
Adhesion to Fruehauf pre-painted panels
3M Controltac™ 3552C Changeable Graphic Film with Comply™ Adhesive
2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to surfaces with corrugations and rivets; Air release channels for fast, easy, bub..
Peel Strength 0.298 kN/m
1.70 pli
Adhesion to Fruehauf pre-painted panels
3M Controltac™ 8652C Changeable Graphic Film with Comply™ Adhesive
Film 8652C is a 2-mil film with sideable, repositionable, pressure-activated adhesive. This short-term durable and removable film is an excellent choice for fleet graphics, including surfaces with c..
Peel Strength 0.298 kN/m
1.70 pli
Adhesion to Fruehauf pre-painted panels
3M Controltac™ IJ3552C Changeable Graphic Film with Comply™ Adhesive
2-mil white, vinyl film; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conformers to surface with corrugations and rivets; Air release channels for fast, easy, bu..