Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.158 kN/m | 0.900 pli | Adhesion to Fruehauf pre-painted panels |
3M Controltac™ 8640C ES Graphic Film with Comply™ Adhesive This 4-mil film offers great versatility along with slidable, repositionable, pressure activated adhesive. This long term durable and removable film has excellent hiding power and stability, making .. |
|||
Peel Strength | 0.158 kN/m | 0.900 pli | Adhesion to Fruehauf pre-painted panels |
3M Controltac™ IJ160C Graphic Film with Comply™ Adhesive 4-mil, opaque white, vinyl film with a matte finish; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Film IJ160C-10 also has Comply™ Adhesive air release channels .. |
|||
Peel Strength | 0.158 kN/m | 0.900 pli | Polypropylene |
3M Fastbond™ 100 Lavender Foam Adhesive 3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t.. |
|||
Peel Strength | 0.158 kN/m | 0.900 pli | Polypropylene |
3M Fastbond™ 100 Neutral Foam Adhesive 3M™ Fastbond™ Foam Adhesive 100 is a one-part, water-dispersed, fast setting adhesive. The neoprene-based product bonds many porous substrates to porous or non-porous substrates with minimal dry t.. |