Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM0186N Clear Polyester Label Products 3M™ Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM023402 Clear Polyester Label Products 3M™ Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM1542 Clear Polyester Label Products 3M™ Clear Polyester Label Products FM1541 and FM1542 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesi.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM1732 White Polyester Label Products 3M™ White Polyester Label Products FM1732 and FM1732R are durable, high performance materials that offer excellent thermal stability. These polyester label products utilize 3M™ Adhesive R3500, whi.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM1732R White Polyester Label Products 3M™ White Polyester Label Products FM1732 and FM1732R are durable, high performance materials that offer excellent thermal stability. These polyester label products utilize 3M™ Adhesive R3500, whi.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP012202 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP0122R2 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP016902 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP0169R2 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP031105 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP0862 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP0863 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP0868 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP0869 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV1220 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV1222 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV1222R Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV1225 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are soft white vinyl label stocks that offer durability and good conformability. These vinyl labels utilize 3M™ Adhesive R3500, which is designed for use on smoo.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM1541 Clear Polyester Label Products 3M™ Clear Polyester Label Products FM1541 and FM1542 are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesi.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP016903 Removable White Polypropylene Label Products 3M™ Removable White Polypropylene Label Products are white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ul.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FP0861 Removable Clear Polypropylene Label Products 3M™ Removable Clear Polypropylene Label Products offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is an ultra removable acrylic designed f.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FM0234R2 Clear Polyester Label Products 3M™ Clear Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These label products utilize 3M™ Adhesive R3500, which is.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV016401 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV016402 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV016405 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV0164R2 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Peel Strength | 0.0526 kN/m | 0.300 pli | 180° Peel, 12"/min., 1" wide sample; TLMI Method |
3M FV016408 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |