Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 560 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
560 g/in @Pressure 40.0 psi, Temperature 266 °F |
Otto Bruger, 0.2 sec; ExxonMobl Method |
ExxonMobil Bicor™ 20MB666 OPP Film Product Description: Bicor 20MB666 is a biaxially oriented transparent polypropylene film acrylic coated two sides. It provides outstanding performance on all packaging machines and is mainly propos.. |
|||
Seal Strength | 560 g/25 mm @Pressure 0.276 MPa, Temperature 130 °C |
560 g/in @Pressure 40.0 psi, Temperature 266 °F |
Otto Bruger, 0.2 sec; ExxonMobl Method |
ExxonMobil Bicor™ 25MB866 OPP Film Product Description: A high speed transparent, biaxially oriented polypropylene film, coated one side acrylic, one side PVOH. It provides excellent gas and aroma protection and is designed to be use.. |
|||
Seal Strength | 560 g/25 mm @Pressure 0.276 MPa, Temperature 140 °C |
560 g/in @Pressure 40.0 psi, Temperature 284 °F |
Otto Brugger, 0.2 sec; ExxonMobil Method |
ExxonMobil Metallyte™ 30MM680 OPP Film Product Description: A biaxially oriented polypropylene film, metalized on one side, heat sealable on the other side. Typically, all gauges are used laminated with other substrates on HFFS and VFFS .. |