Seal Strength <= 3000 g/25 mm
<= 3000 g/in
PP, bar temp 150-200°C
DuPont Appeel® LSR 11D569 Modified EVA Lidding Sealing Resin  (discontinued **)
Appeel 11D569 is a modified ethylene vinyl acetate copolymer resin designed to be used as a sealing layer for lidding applications. It provides peelable seals to a variety of surfaces including poly..