Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Seal Strength = 2800 g/25 mm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Seal Strength 2800 g/25 mm
2800 g/in
F-88-68(73)
DuPont™ Clysar® EHC Polyolefin Shrink Packaging Film, 75 Gauge  (discontinued **)
Data provided by DuPont Packaging Polymers.A biaxially oriented, heat-shrinkable copolymer film. It is a polypropylene and polyethylene-based film that is predominantly polypropylene. Used when exc..
Seal Strength <= 2800 g/25 mm
<= 2800 g/in
Varies with seal bar temp.
DuPont™ Surlyn® 1855 Zinc Ionomer Resin for Blown and Cast Film  (discontinued **)
Surlyn® 1855 is an ionomer resin available for use in conventional blown and cast film extrusion and coextrusion equipment designed to process polyethylene resins. Applications: Meat, poultry, sea..
Seal Strength 2800 g/25 mm
2800 g/in
seal bar 125°C.
DuPont Nucrel® 0609HS Ethylene-Methacrylic Acid Copolymer Resin for Extrusion Coating/Laminating  (discontinue
6 wt% Methacrylic Acid.Nucrel® 0609HS* (High-Speed) is an ethylene-methacrylic acid copolymer resin available for use in conventional extrusion coating, coextrusion coating, and extrusion laminatin..
Copyright © lookpolymers.com All Rights Reserved