Mechanical Properties Metric English Comments
Seal Strength 260 g/25 mm

@Pressure 0.276 MPa,
Temperature 130 °C
260 g/in

@Pressure 40.0 psi,
Temperature 266 °F
Otto Bruger, 0.2 sec; ExxonMobl Method
ExxonMobil Bicor™ 25MB666 OPP Film
Product Description: A Biaxially oriented transparent polypropylene film, acrylic coated two sides. It provides outstanding performance on all packaging machines.Availability: Africa & Middle East, ..