Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Seal Strength | 1800 - 2400 g/25 mm | 1800 - 2400 g/in | Average value: 2070 g/25 mm Grade Count:12 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Film Grade". Each property range of values reported is minimum .. |