Polymer Property : 1% Secant Modulus, TD = 931 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 931 MPa
135000 psi
ASTM D882
Lotte Chemical Titan TITANEX® HF1881 High density polyethylene Hexene-1 resin
HF1881 is a pelleted medium molecular weight, high density polyethylene Hexene-1 resin for tubular film extrusion.Applications: Grocery sacks, shopping bags, liners and thin films.Advantages: Speci..