Polymer Property : 1% Secant Modulus, TD = 85600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 590 MPa
85600 psi
ASTM D882
Chevron Phillips K-Resin® KR53 Styrene-Butadiene Copolymer
Customer Benefits:Excellent ClarityHigh Surface GlossGood ToughnessGood Heat SealabilityTypical Applications:Medical PackagingProduce PackagingTwist WrapLidstock and Labeling FilmInformation provide..