Polymer Property : 1% Secant Modulus, TD = 7250 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 50.0 MPa
7250 psi
ISO 527-3
Polimeri Europa Clearflex® CL D0 Very Low Density Polyethylene
Clearflex CL D0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).This resin is produced with a proprietary technology. Stretch films manufactured..