Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 49.0 MPa | 7100 psi | ASTM D882 |
Westlake EMAC® SP2252 20.5% Ethylene-Methyl Acrylate Copolymer Westlake EMAC® SP2252 is a 20.5% EMA copolymer containing slip and antiblock. This resin is designed for blown film, tie-layers, and extrusions where flexibility, compatibility, or low heat seal te.. |