Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 60.4 MPa | 8760 psi | ASTM D882 |
ExxonMobil OPTEMA™ TC 115 Blown Film Resin
(discontinued **) OPTEMA TC 115 is an ethylene methyl acrylate copolymer, designed for specialty blown film applications. It yields soft, elastic films.Information provided by ExxonMobil Chemical |