Mechanical Properties Metric English Comments
1% Secant Modulus, TD 345 MPa
50000 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308DK Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD..
1% Secant Modulus, TD 345 MPa
50000 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308DL Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processingIncreased stiffnessGood toughnessUse alone or in blends with LDPE or HD..
1% Secant Modulus, TD 345 MPa
50000 psi
Blown Film at 1 mil; ASTM D-882
Chevron Phillips MarFlex® 7308FK Polyethylene; LLDPE
Hexene linear low density polyethylene. This LLDPE is tailored for blown film applications that require: Excellent processabilityIncreased stiffnessGood toughnessUse alone or in blends with LDPE o..
1% Secant Modulus, TD 345 MPa
50000 psi
ASTM D882
ExxonMobil Enable™ 27-05CH Metallocene Polyethylene Resin (European Grade)
Product Description: Enable 27-05CH is a metallocene ethylene-hexene copolymers. Enable mPE resins offer an outstanding balance between processing and film properties, including tensile, impact and ..
Copyright © lookpolymers.com All Rights Reserved