Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : 1% Secant Modulus, TD = 37200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 256 MPa
37200 psi
ASTM D882
ExxonMobil LD 103.MP Industrial Film Resin  (discontinued **)
LD 103 resins are homopolymer industrial film resins are used in box and drum liners, industrial packaging, medium duty shrink wrap, construction and agriculture film, and rubber bale wrap.Informati..