Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
ExxonMobil LD 136.MV Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
ExxonMobil LD 136.NI Packaging Film Resin
(discontinued **) LD 136 series resins are homopolymer film resins with good clarity. They are suitable for processing in cast film equipment. Applications include food packaging, textile packaging, and other packa.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D638 |
LyondellBasell Petrothene® GA502022 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D638 |
LyondellBasell Petrothene® GA502024 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D638 |
LyondellBasell Petrothene® GA502023 Linear Low Density Polyethylene ApplicationsThe PETROTHENE GA 502 series of resins are pelletized linear low density polyethylene for film extrusion applications requiring excellent drawdown and toughness. These pelletized produc.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
Westlake EF706 Low Density Polyethylene Westlake EF706 is a high melt index LDPE resin suggested for thin gauge garment films and other films requiring excellent drawdown. The high melt index makes this material a good choice in compound.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
Westlake LF1050 Butene Linear Low Density Polyethylene Westlake LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or MDPE.Application/UsesCast film extrusionPr.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
Westlake LF2020 Hexene Linear Low Density Polyethylene Westlake LF2020 is a hexene LLDPE with excellent physical properties and heat sealing characteristics, which allow for down-gauging and blending with other materials. Typical applications include s.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
ExxonMobil LD 143.26 High Clarity Packaging Film Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
1% Secant Modulus, TD | 248 MPa | 36000 psi | ASTM D882 |
ExxonMobil LDPE LD 159AC Low Density Polyethylene Resin Product Description: LD 159AC is an LDPE grade, which offers good draw down combined with good mechanical strength. Availability: Africa & Middle East and Europe Additive: Antiblock: 450 ppmSlip: 5.. |