Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 338 MPa | 49000 psi | ASTM E111 |
LyondellBasell Petrothene® L3035 Low Density Polyethylene, Film Extrusion Grade Petrothene L3035 is a fractional melt index LDPE resin that exhibits an exceptional balance of optics, modulus, puncture, tear and shrink characteristics. Typical applications include collation shri.. |