Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 300 MPa | 43500 psi | ASTM D882 |
SABIC 6821N Linear Low Density Polyethylene for Blown Film Product Description: 6821N is a fractional melt index hexene copolymer based Linear Low Density Polyethylene grade suitable for high strength packaging applications. Films produced using this resi.. |