Mechanical Properties Metric English Comments
1% Secant Modulus, TD 28.3 MPa
4100 psi
ASTM D882
Westlake EMAC® Plus SP1358 21.5% Ethylene-Methyl Acrylate Copolymer
Westlake EMAC® Plus SP1358 is a 21.5% EMA copolymer containing slip and antiblock. This resin is designed for blown or cast film, tie-layers, and extrusions where flexibility, compatibility, or low..