Polymer Property : 1% Secant Modulus, TD = 23400 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
1% Secant Modulus, TD 161 MPa
23400 psi
ASTM D882
ExxonMobil LD 317.09 Film Resin
LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon..
1% Secant Modulus, TD 161 MPa
23400 psi
ASTM D882
ExxonMobil LD 317.87 Film Resin
LD 317 Series offer excellent impact strength, tensile properties, and heat sealability. Applications include ice bags, frozen food packaging, and other food packaging.Information provided by Exxon..