Mechanical Properties Metric English Comments
1% Secant Modulus, TD 225 MPa
32600 psi
ISO 527-3
Polimeri Europa Clearflex® FG 306 Hexene Copolymer Linear Low Density Polyethylene
Clearflex FG 306 is a hexene copolymer linear low density polyethylene (C6-LLDPE), with antioxidant, antiblocking and processing aid, suitable for blown film extrusion.Films manufactured with Clearf..