Mechanical Properties Metric English Comments
1% Secant Modulus, TD 205 MPa
29700 psi
ASTM D 882
NOVA Chemicals Sclair® FP020-D Octene Copolymer LLDPE Film Resin
FP020-D complies with the U.S. FDA specifications for olefin polymers and may thus be used in the United States as an article or component of an article intended for use in contact with food. FP020..
1% Secant Modulus, TD 205 MPa
29700 psi
ASTM D882
ExxonMobil Exceed™ 1018CA Premium Blown Film Resin  (discontinued **)
Exceed 1018CA is a hexene copolymer produced using ExxonMobil Chemicals EXXPOL® Technology. Films made from 1018CA have outstanding tensile, impact strength and puncture. These superior strength ..