Mechanical Properties | Metric | English | Comments |
---|---|---|---|
1% Secant Modulus, TD | 1270 MPa | 184200 psi | ASTM D882 |
NOVA Chemicals Sclair® 19G Homopolymer HDPE Film Resin Features: Excellent barrier propertiesHigh stiffnessGood processability Low gel Applications: Barrier filmsCo-extrusionDry food packagingInformation provided by Nova Chemicals |